of a through thickness crack two times (2X) the wall thickness, or a size agreed upon with the Procuring Service, when subject to limit loading conditions.
d. proof testing concept where a pressurization test is performed on each production component that can effectively demonstrate that the part is damage-tolerant. The pressure level at which this testing is performed must be supported by analysis to document exposure to the specified proof pressure level confirms damage tolerance of the part/assembly.